We have manufactured vessel as per ASME Sec VIII Div. 1.
This vessel is partly manufactured at shop & final assembly /
hydrotest carried at field.
My organization is having ASME U stamp certificate of authorization &
socpe covering
shop & field activities.
My question is while moving out semi finished vessel from shop to
field whether
Manufacturers Partial Data Report is required?
Field assembly & testing will be completed by same organization.

Experts / ASME Authorized Inspector's views are requested.

Thanks!

Arunachalam A

unread,
Oct 21, 2010, 12:33:43 PM10/21/10
to material...@googlegroups.com
Use U1 form and get it signed by AI in the place meant for shop inspection.
After field erection and hydrostatic test witnessed by AI, the certificate of field inspection shall be signed by AI.

Arun


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


Shashank Vagal

unread,
Oct 22, 2010, 8:26:40 AM10/22/10
to material...@googlegroups.com
Yes, you can first make a PDR, get it signed by the AI; after field assembly  complete it all with an MDR using your PDR as a back up, get it signed by the AI. In all respects, this will be the best, eliminating any ambiguities in future by accounting for stage wise fabrication and inspection and certification by the AI..