Kindly advice whether we can use 99.99% Ar gas for welding of FCAW process on carbon steel,as one of our customers is insisting for the same, we have informed them that it is not possible as there will fusion problems,also the weld will not be sound weld. Pure Argon can be  used for welding of Stainless steel, aluminium.

Please provide  some interpretation or code reference through which we can convince client.

Thanks & Regards,
Anthony. 

dilintas

unread,
Nov 18, 2016, 9:59:23 PM11/18/16
to Meghanadh K
In many occasions I have pointed out that the Code is not a hand book. You will look for in vain to find such a recommendation in the Code.
The best tool is the filler metal manufacturer's recommendation and the AWS prequalified WPSs



Sent from my Samsung Galaxy smartphone.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-WQZEzLYTv2-4H5aX_W-BM%3DwwTWavOT9CDBNCKCQBjNw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages