Mechanical Values of A269 TP304 Seamless tubes

61 views
Skip to first unread message

ppe...@gmail.com

unread,
Oct 19, 2010, 2:27:49 AM10/19/10
to material...@googlegroups.com
Dear All,
Please help me to find that what is the mechanical test required in A269 TP304 Seamless tubes. What are the tensile requirement of tubes.
Thanks and Regards
S Malik
Sent on my BlackBerry® from Vodafone

hpi001

unread,
Oct 19, 2010, 4:08:25 AM10/19/10
to Materials & Welding
Dear Mr. Malik,

I tried to find any specification called ASTM A269 but couldn't find
it, its also not mentioned in Section II part A of ASME IIIV as SA269.
Is the specification mentioned correct and still current?

Best Regards,

Herman Pieper

Karthik

unread,
Oct 19, 2010, 4:27:08 AM10/19/10
to material...@googlegroups.com
Hi,
SA269 TP304(UNS No.S30400) is not listed in ASME It has been replaced to SA312 TP304(UNS No.S30400). The material properties of this type of steel is define by this grade.In this case (SA269 TP304) is a SEAMLES AND WELDED AUSTENITIC STAINLESS STEEL TUBING FOR GENERAL SERVICE.You can get the properties of this material as specified in SA312 TP304.
 
Please find below the Properties of TP304.
Tensile Strength: 75Ksi(515MPa)
Yield Strength: 30Ksi (205MPa)
 
Note:
Mechanical property requirements do not apply to tubes smaller than 1/8. (3.2mm) in in side diameter or 0.015 in.(0.38mm) in thickness
 
For test requirements pls.refer to SA312 and A999
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 10/19/10, hpi001 <piepe...@kpnmail.nl> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Reply all
Reply to author
Forward
0 new messages