AWS D1.1 Table 4.6 Clause 1-Change in Group No.

1,078 views
Skip to first unread message

K.Babu

unread,
Jul 24, 2011, 9:55:29 AM7/24/11
to material...@googlegroups.com
Gents,
 
 
WPS is qualified in Group II to Group II, with CVN @-40 deg. cel.,
 
Can we use this WPS , to weld Group II to Group I  combination with requirement of CVN @-20 deg cel.
 
 
Thanks & regards,

K.Babu

Rems Okonkwo

unread,
Jul 25, 2011, 8:25:37 AM7/25/11
to material...@googlegroups.com
Dear K Babu,

WPS qualified on group II materials can be use on group I and Group II and its combination if all other variables are constant.
As per the CVN @-40, if the values obtained @-40 met the specification requirement @ -20 then the WPS is qualified as you requested. so you need to check the minimum value required @-20 and if the values obtained @ -40 meet the requirement @-20.

Regards,

Rems Okonkwo

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

KINHUI KANG

unread,
Jul 25, 2011, 10:34:10 AM7/25/11
to material...@googlegroups.com
Dear K.Babu,

A change in Group Number is a supplementary essential variable according to AWS D1.1.
Your WPS qualified in Group II to Group II cannot qualify for Group I to Group II.

Best regards,
Kang


Date: Mon, 25 Jul 2011 13:25:37 +0100
Subject: Re: [MW:11906] AWS D1.1 Table 4.6 Clause 1-Change in Group No.
From: rems.o...@gmail.com
To: material...@googlegroups.com

Eswaran samikannu

unread,
Jul 25, 2011, 10:47:17 AM7/25/11
to material...@googlegroups.com
As Per AWS D1.1 Group 2 material qualifies Group 1 also & CVN -40 Qualifies -2o also.

By
S.Eswaran
CSWIP -3.2.1
ASNT NDT Level III (RT,UT,PT &MT) 


From: K.Babu <kbab...@gmail.com>
To: material...@googlegroups.com
Sent: Sunday, 24 July 2011 9:55 PM
Subject: [MW:11886] AWS D1.1 Table 4.6 Clause 1-Change in Group No.

manpreet

unread,
Jul 25, 2011, 10:32:13 PM7/25/11
to material...@googlegroups.com
Hi,
 
Unfortunately you can not use PQR (P1 Gr2 to P1 Gr2) to weld P1 Gr1 to P1 Gr2, find out if you have PQR qualified with P1 Gr1 to P1 Gr2.
 
Intent of code is to have impact test done on both material else look for a material with dual certificate (both Gr1 & Gr2).
 
 
Regards
Manpreet Singh
 


From: "K.Babu" <kbab...@gmail.com>
Sent: Tue, 26 Jul 2011 07:53:34
To: material...@googlegroups.com
Subject: [MW:11886] AWS D1.1 Table 4.6 Clause 1-Change in Group No.
Gents,
 
 
WPS is qualified in Group II to Group II, with CVN @-40 deg. cel.,
 
Can we use this WPS , to weld Group II to Group I  combination with requirement of CVN @-20 deg cel.
 
 
Thanks & regards,

K.Babu

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

K.Babu

unread,
Jul 26, 2011, 7:17:50 AM7/26/11
to material...@googlegroups.com

Manpreet,
 
Sec IX not in picture .
--
Thanks & regards,

K.Babu
Singapore