Prequalified WPS Essential variables for AWS D1.1 Table3.7 with Table 4.1&4.2

127 views
Skip to first unread message

QC Engineer

unread,
Sep 20, 2020, 11:37:59 PM9/20/20
to Materials & Welding
Dear Experts,

As per the PWPS essential variables given in Table 3.7 -23 of AWS D1.1,
and comparing it with Table 4.1&4.2,is it permitted to use the Prequalified WPS made for Butt joint welding for FIllet welding also.?


Table 4.1 &4.2 is applicable to Prequalified WPS or not?

Regards



Raja Varman

unread,
Sep 21, 2020, 12:33:03 AM9/21/20
to material...@googlegroups.com
Table 3.7 is for pwps
Table 4.1 & 4.2 - WPS requirements.

Both scope the std have different table of essential variables.

So. You must prepare one pwps for fillet.
2015 edition have seperate joint configuration for fillet joints in PWPS.



என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70d11f92-f4e5-4719-8604-9131eb30b698o%40googlegroups.com.

Vinay Thattey

unread,
Sep 21, 2020, 11:12:30 PM9/21/20
to material...@googlegroups.com, bino...@gmail.com
No