Crack in Duplex S.S material

92 views
Skip to first unread message

ABHISHEK SINGH

unread,
Jan 27, 2015, 6:29:23 AM1/27/15
to material...@googlegroups.com
Dear Experts,
We got longitudinal crack on material SA240UNS31803 (D.S.S material).This is found after RT.Following consumable we used: Wire-ER2209,Flux-15W(Sandvik).

Please share your experiance regarding this.

Thanks & Regards
Abhishek

Jian Xu

unread,
Apr 12, 2015, 11:18:02 PM4/12/15
to material...@googlegroups.com


Dear Abhishek,

Maybe you should check the whole welding process whether is corrdance with WPS . And you can do some basic test for the failure part, such as ferrite content.
To confirm root cause, then identify which welding process generate impact.

Thanks
Leon 

Jim Price

unread,
Apr 13, 2015, 10:55:12 PM4/13/15
to material...@googlegroups.com

What grade of duplex are you welding?

Lean or Super governs the amount of heat input allowed.

What welding process are you using? What shielding gas are you using?

 

Jim

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0969469b-fb7a-45b0-ab1d-515fbcad38c7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Ramin Kondori

unread,
Apr 14, 2015, 7:12:07 AM4/14/15
to material...@googlegroups.com
Dear Abhishek

Please provide us with more info as following:

  1. When did crack appear (immediately after welding or after a couple of days or in service...?)
  2. A photo of the crack (is the crack in weld of HAZ...?)
  3. Is the crack in root side of face...?
  4. Thickness of material
  5. Heat input during welding (KJ/mm)
  6. Did you control inter-pass temp...?
  7. Did you use any gas for back purge...?