Dear All

What is the ASTM/ASME equivalent of structural material S355J2+N (minimum yield strength 355 MPa, Tensile 470 to 630 MPa, C: 0.20 max, Si: 0.55 max, Mn: 1.60 max , CE: 0.45 max). A link to reference document stating the same would be much appreciated.

Thanks & best regards

Kathalingam Babu

unread,
Apr 26, 2011, 4:24:40 AM4/26/11
to material...@googlegroups.com
ABS Grade EH36
Also, ASTM A131 Gr.EH36
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Elshan Feyzullayev

unread,
Apr 26, 2011, 5:19:29 AM4/26/11
to material...@googlegroups.com
A516 Gr70 is ok to substitute.
 

From: kathalin...@ppl.com.sg
To: material...@googlegroups.com
Subject: Re: [MW:10856] ASME/ASTM equivalent of S355J2+N
Date: Tue, 26 Apr 2011 16:24:40 +0800

Cheril Rajeev

unread,
Apr 26, 2011, 5:36:20 AM4/26/11
to material...@googlegroups.com
Equillent material for S355JR+N  is ASTM A 572. But Y.S (345) and T.S is lesser than S355JR.
 
Regards
Cheril

--

SENTHILKUMAR SWAMINATHAN

unread,
Apr 26, 2011, 8:44:04 AM4/26/11
to material...@googlegroups.com
Vikas,
Refer attached may help you. Hope it is A36 (ASTM)
 
Regards,
S.SENTHILKUMAR



From: Vikas Bhandari <vikas.bh...@gmail.com>
To: material...@googlegroups.com
Sent: Tue, 26 April, 2011 9:09:50 AM

Subject: [MW:10855] ASME/ASTM equivalent of S355J2+N

Dear All

What is the ASTM/ASME equivalent of structural material S355J2+N (minimum yield strength 355 MPa, Tensile 470 to 630 MPa, C: 0.20 max, Si: 0.55 max, Mn: 1.60 max , CE: 0.45 max). A link to reference document stating the same would be much appreciated.

Thanks & best regards

--
catalogue_of_plates_new S355.pdf

Kathalingam Babu

unread,
Apr 26, 2011, 8:30:03 PM4/26/11
to material...@googlegroups.com
Senthil
 
A36 doesn't have any Impact requirement, But S355K2+N is need an CVN@-40 deg cel.
 
Thanks & Regards,
 
K. Babu
----- Original Message -----

Kathalingam Babu

unread,
Apr 26, 2011, 8:32:11 PM4/26/11
to material...@googlegroups.com
Sorry , CVN @-20 deg.cel
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
Sent: Tuesday, April 26, 2011 8:44 PM
Subject: Re: [MW:10863] ASME/ASTM equivalent of S355J2+N

Arunachalam A

unread,
Apr 26, 2011, 2:13:40 PM4/26/11
to material...@googlegroups.com
It is NOT ASTM A36. A36 has specified tensile of 420 N/mm2.
--
Arunachalam.A,
Abu Dhabi Gas Industries Ltd,
P.O.Box # 50124
Abu Dhabi, UAE

Muhamad Zuhdey Sharifudin

unread,
Apr 26, 2011, 11:28:23 PM4/26/11
to material...@googlegroups.com, material...@googlegroups.com

S355j2+N is normalized supply condition material have impact cvn -40 deg..

ASTM A36 is as rolled material w/o any impact req


Arunachalam A <arun...@gmail.com>
Sent by: material...@googlegroups.com

04/27/2011 02:13 AM


To
material...@googlegroups.com
cc
Subject
Re: [MW:10867] ASME/ASTM equivalent of S355J2+N


Mrityunjay Kumar / ZS Saudi PEB QA/QC

unread,
Apr 27, 2011, 12:35:36 AM4/27/11
to material...@googlegroups.com

Dear Vikas,

The ASTM/ASME equivalent of structural material S355J2+N is ASTM A572 Gr-50

 

Best Regards,

M.K.Choudhary

cid:image001.gif@01C5934C.F0F5DF10

P.O. Box 877,  Dammam  31421  KSA

Phone  : (+9663) 8471840 X 555

Fax       : (+9663) 8471291

www.zamilsteel.com

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Arunachalam A
Sent: Tuesday, April 26, 2011 9:14 PM
To: material...@googlegroups.com
Subject: Re: [MW:10867] ASME/ASTM equivalent of S355J2+N

 

It is NOT ASTM A36. A36 has specified tensile of 420 N/mm2.

--------------------------------------------------------------------------------------------------------
Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use, disseminate,
distribute, copy or alter this email. Any views or opinions presented in this
email are solely those of the author and might not represent those of "Zamil
Industrial" and or its units.

Warning: Although reasonable precautions have been taken to ensure no viruses
are present in this email, the company cannot accept responsibility for any
loss or damage arising from the use of this email or attachments. If you have
received this electronic mail message in error, please contact the sender directly.

Plate Steel

unread,
Oct 21, 2015, 4:02:19 AM10/21/15
to Materials & Welding
S355J2+N under EN 10025-2 need Normalized plus low temperature impacting test under -20 centigrade.

So If using ASTM A572Gr50,you have to ask additional techincals requirements (Normalized heat treatment,-20 Centigrade low temperature impacting test),then this A572Gr50 steel shall be equal to S355J2+N.

Also,ship plates A131 Grade DH36 and A131 Grade EH36 is also equal to S355J2+N and even better than S355J2+N.

Hope this would be useful to you.

Eric from Xinsteel Industrial Co.,Limited