Interpretation QW202.2 b

109 views
Skip to first unread message

SANJAY SINGH

unread,
Nov 24, 2023, 6:58:55 AM11/24/23
to material...@googlegroups.com
Dear One and All ,
               Please let me know QW 202 .2 b  actual interpretation  for partial penetration .

I have WPS  with Base metal thickness of 40 mm then whether it qualifies for partial weld groove above 200 mm Thk. base metal thickness also .

image.png



Regards 
Sanjay 

Vishwas Keskar

unread,
Nov 24, 2023, 10:34:22 AM11/24/23
to material...@googlegroups.com
40 mm PQR test coupon 
Then there is no limit for partial penetration groove welding  base metal thickness limitation
Sent from my iPhone

On 24-Nov-2023, at 5:28 PM, SANJAY SINGH <sanjay.k...@gmail.com> wrote:


Dear One and All ,
               Please let me know QW 202 .2 b  actual interpretation  for partial penetration .

I have WPS  with Base metal thickness of 40 mm then whether it qualifies for partial weld groove above 200 mm Thk. base metal thickness also .

<image.png>




Regards 
Sanjay 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALkBf%2Bvnq_Vf5cGmGMoLe99grjVwvGZt%2BvRUxip50bgitDHtDQ%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Nov 24, 2023, 10:34:23 AM11/24/23
to materials-welding
yes, Maximum to be welded because test coupen thickness is 40mm

--