Hi welding experts ,

I want to do a welding procedure in accordance to ISO15614, the client material rance from 16mm to 40mm, making reference to take table 7 of ISO15614, would using a 20mm plate support the qualification of the material thickness in question? most especially the 40mm 

--
RILLEY CHELLAH MULENGA
Materials Evaluation Head of Department
E: rilley....@ahkgroup.com
CompanyLogo
 


DISCLAIMER: The information in this Internet e-mail is confidential and may be legally privileged. It is intended solely for the addressee(s).
Access to this Internet e-mail by anyone else is unauthorised.

If you are not the intended recipient, any disclosure, copying, distribution or any action taken or omitted to be taken in reliance on it, is prohibited and may be unlawful.
All results and data contained in this document are subject to our Standard Terms and Conditions and are valid only when supported by an original document.

Please visit our website at www.ahkgroup.com
table 7 iso 15614.png

bavithran samuthralingam

unread,
Apr 15, 2026, 8:27:13 AMApr 15
to material...@googlegroups.com
Hi 
You can select a test piece of 25 mm so that u can get a thickness range from 12.5 mm to 50 mm range 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHkXHT-4ht_Fd6hUr6doAzU061UEvQtsRaRn--KVd0aHgELgiw%40mail.gmail.com.

Rilley Chellah Mulenga

unread,
Apr 15, 2026, 9:48:26 AMApr 15
to material...@googlegroups.com
Hi bavithran samuthralingam,

Using a 20mm plate will be too tight for the procedure right ? since it will be borderline  nowonder you suggest 25mm ? very interesting 


Edvinas Jonas

unread,
Apr 15, 2026, 1:38:09 PMApr 15
to material...@googlegroups.com

Hi,

yes, 25 mm seems to be the safer option since it qualifies the 12.5–50 mm thickness range.

20 mm would be more borderline for our target range.