Distance b/w branch weld and pipe seem weld

76 views
Skip to first unread message

Mahmood Al-Hinai

unread,
Nov 30, 2022, 12:42:12 AM11/30/22
to material...@googlegroups.com
Experts,

What is the requirement for the distace between branch weld and pipe seem weld. 
Is the condition in attached photo accepted or not?
Pls advise

Thanks
Mahmood
IMG-20221130-WA0004.jpg

chipfr...@gmail.com

unread,
Nov 30, 2022, 10:18:34 PM11/30/22
to material...@googlegroups.com

What is the code of construction?

Many codes do not address this issue.

If it is not prohibited by specification, then it should be acceptable.

 

 

 

Thanks,

 

 

Chip Frizzell

 

CWI / ASNT NDT Lvl III / CRI / NACE CIP Lvl 2 – Certified

 

chipfr...@gmail.com

CELL: 520-510-8093

 

Price is what you pay – Value is what you get.

Seldom does the lowest price result in the best value!

 

Integrity . Satety . Respect

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEuX%2Bdk%2BkMiraG4-1YmWuRhwrgCLczaPZYgvpUGVyEoQV00jmA%40mail.gmail.com.

Yunsok Bang

unread,
Nov 30, 2022, 10:18:34 PM11/30/22
to material...@googlegroups.com
Hello.


This link will help your question.

In my work place follow the BS code. The 4t(nominal pipe thickness).

Have a good day.

--

Ritesh Kumar Singh

unread,
Dec 1, 2022, 4:10:46 AM12/1/22
to material...@googlegroups.com
Depends on code and specifications as I remember in B31.3 it is  5T( wall thickness of pipe*5).


G Gughan

unread,
Dec 1, 2022, 4:45:10 AM12/1/22
to material...@googlegroups.com

Dear Mahmood,

          There is no clear quote for minimum weld distance length in ASME B31.1 Power piping standards, where there is minor guidance provided for a few locations as mentioned below:

1.    131 WELDING PREHEAT:

image.png


2.    Figure 104.3.1-1 Reinforcement of Branch Connections (Cont’d)

image.png


3. Table D-1 Flexibility and Stress Intensification Factors (Cont’d)

image.png


General Note: In the cross-country pipeline, to maintain a minimum weld distance length is so difficult in a position of mitre elbow. Your weld should have integrity as mentioned in the specs. Use any type of NDE.

Olets fittings welds shall be carried out by the approved WPS. If there is no condition mentioned in your contract. You can waive it. 


Thanks,