Electrode Qualification Test requirement

224 views
Skip to first unread message

mohan raj v

unread,
Sep 30, 2015, 12:10:00 AM9/30/15
to Materials & Welding
Dear All, 

Please clarify for electrode qualification test as per ASME Sec II Part C for E7018 Dia-4 mm, what are the test requirements?.
As per Table 4, Fillet weld test piece is required for chemical analysis, RT, All-weld test & Impact test. Please clarify what table 4 is stating.

Further, if i make one Groove weld test assembly of 20 mm thick, is it sufficient for the electrode qualification?

Thanks & Regards,

Mohan Raj 

CHINTUKUMAR GANDHI

unread,
Sep 30, 2015, 3:49:45 AM9/30/15
to material...@googlegroups.com
Dear member,

Table-4 of SFA 5.1 of ASME Sec. IIC is for the tests required. You will have to refer SFA 5.1 in depth to comply those tests.

Thanks & regards,

C. R. Gandhi


From: mohan raj v <vmra...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Tuesday, September 29, 2015 11:34 PM
Subject: [MW:23618] Electrode Qualification Test requirement

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/021aa57f-3ee7-4f7f-98f5-e43c1122d570%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


RAJENDRA PRASAD TRIPATHI

unread,
Oct 6, 2015, 8:10:52 AM10/6/15
to Materials & Welding
Generally  RT ,All weld-test with impact and one chemical pad is sufficient 