Hardness Value of Inconel 625

482 views
Skip to first unread message

LALU RAJENDRAN

unread,
Dec 31, 2014, 11:11:46 PM12/31/14
to material...@googlegroups.com
Dear Experts,

What is the hardness value of Inconel-625 (ASTM B444 UNS N06625)?


Regards,
LALU
LINKS MIDDLE EAST

nithind...@gmail.com

unread,
Jan 9, 2015, 12:19:51 AM1/9/15
to material...@googlegroups.com
Hi,

It is not specified in code, if you refer to shell MESC, it is 32 HRC.

Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13t1W3GvM2xV6z3_D91J-DiUjTgwynS%3DL3qeCBOTPy2-Ng%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Shridev Kurup

unread,
Jan 9, 2015, 10:01:11 AM1/9/15
to material...@googlegroups.com

345 HV max

--

Vairamuthu Ramar

unread,
Jan 9, 2015, 11:27:44 PM1/9/15
to material...@googlegroups.com
hi,
 
as per NACE MR0103-2005, it is 35HRC.
 
I have attached snapshot of the standard. Pls refer the attachment and correct me if i am wrong.
 
Regards
R Vairamuthu
 

 

Subject: Re: [MW:22691] Hardness Value of Inconel 625
From: nithind...@gmail.com
Date: Fri, 9 Jan 2015 08:32:05 +0400
To: material...@googlegroups.com
NACE MR0103 - 2005.docx

Vairamuthu Ramar

unread,
Jan 10, 2015, 5:18:05 AM1/10/15
to LALU RAJENDRAN, material...@googlegroups.com
Hi,
 
Pls find the attached hardness conversion table.
 
as per this 35 HRC = 345 HV.
 
For vickers hardness tesing the surface finsih is more important. pls refer std ASTM E92 for specimen prep. and surface finish of the specimen. Even slight variation in surface prep. may lead to wrong measurement.
 
 
Regards
 
Vairamuthu R.

 

Date: Sat, 10 Jan 2015 11:03:02 +0400

Subject: Re: [MW:22691] Hardness Value of Inconel 625
From: lal...@gmail.com
To: vairam...@hotmail.com; material...@googlegroups.com

Dear All,

Thank you for your valuable comments. I am getting an average value of 376 HV10 on HAZ & parent metal side of my PQR test coupon(ASME SEC IX). Should I reject the test coupon...?


​regards,