As I received a inquiry recently, our customer insist to use BS221-6061 fin material for A179 EXTRUDED - SERRATED FIN TUBE. But our factory suggests to use  BS221-6063, as they thought 6061 is too hard to weld. Could you give some suggestion about whether 6061 could be fin material? 企业微信截图_17576437773495.png

sridhar cn

unread,
Sep 12, 2025, 1:57:30 AMSep 12
to material...@googlegroups.com

BS221-6061 has a higher tensile strength and is generally stronger than 6063. From a weldability point, 6061 can 

lead to issues such as cracking if not handled properly during the welding process.


BS221-6063 is easier to weld and has lower strength than 6061; it is often sufficient for applications where extreme 

strength is not a primary concern.


If the customer insists on 6061, specify a soft tempered 6061-O or 6061-T4, confirm with the fin manufacturer that 

their serrating/rolling equipment and process can handle 6061 without cracking.


C Sridhar.


On Fri, 12 Sept 2025 at 09:34, 汪梦佳 <mia_yuh...@foxmail.com> wrote:
As I received a inquiry recently, our customer insist to use BS221-6061 fin material for A179 EXTRUDED - SERRATED FIN TUBE. But our factory suggests to use  BS221-6063, as they thought 6061 is too hard to weld. Could you give some suggestion about whether 6061 could be fin material? 企业微信截图_17576437773495.png

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/5c979648-bb1a-41c1-9c5c-d5ebab7e6024n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages