Dear experts
We are repairing EN GJS 400-15(DIN EN 1563) casting with ENiFe-CI Aws 5.15 electrode. Now customer is asking for repair wps and pqr of the same. What will be the P no of casting and F no And A no of welding consumale. In Asme sec ix only aws 5.14 is mentioned. There is no clue of 5.15. Kindly help me to find it.