316L full rust due to acid attact

30 views
Skip to first unread message

S.Mohammed

unread,
Apr 12, 2015, 11:19:47 PM4/12/15
to material...@googlegroups.com
Dear all,

What is opinion? 316L piping facing full rusted due to acid fumes.HCL.
It is not going by pickling also.
Any solution? For prevention.

Hareesh K V

unread,
Apr 13, 2015, 10:54:13 PM4/13/15
to materials-welding

Dear sir

FRP coating on the SS pipe will solve this issue.

Best Regards

HAREESH K V

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b8ad6890-065e-4c28-a776-2af6f910c994%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Asif Raza

unread,
Apr 14, 2015, 7:12:55 AM4/14/15
to material...@googlegroups.com

Dear send pictures and your inspection report at my email.

 

 

Peter

Welding Engineer