Dear Experts,
Good Morning,
We are having our own project to build an offshore jacket for a depth of 15 to 20 meter water depth. For this project we are in the stage to order the material (PIPE) from the Steel Mill. In order to start the process the mill is asking for the SPEC of PWHT. So can anyone able confirm what should be the Holding temp / time / No of cycle / Stress relieving cycle required for PWHT.
|
Sl.No |
Material Size |
Grade |
Remark |
|
1 |
24" Pipe x 25mm wall thick |
API 5L Gr.X52N PSL2 |
Normalizing Steel |
|
2 |
30" Pipe x 30 mm wall thick |
API 2H GR.50 +(Z35) |
Normalizing Steel |
|
3 |
20" Pipe x 25mm wall thick |
API 5L Gr.X52M PSL2 |
TMCP Steel |
Regards
Thandesh
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABatnw_-jRk6uM_CiFVFgT5YQHSQM1FuWRsV6kzykJPWhUVQeQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AbqQyfQSbN_fys9W1cjjv%3D4tTTyoHroQEoiXu%2BXkbsvg%40mail.gmail.com.