Dear expert,

  Could you please give us your feedback & return experience about impact of PWHT (Heat treatment in general) in defect.

Could  size of porosity (volumic defects) can change after PWHT especially for ally steels ?
Any information for surfacic defects ?

Could you please confirm and give us some reference from codes and/or litterature.

Thank you very much.

--

Thanks and Regards, 
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

George Dilintas

ungelesen,
27.11.2016, 21:46:0827.11.16
an Meghanadh K
Not at all unless you "burn" it

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB252bTKqszekuaTvYBKSJcuLQ%3DU2c_gRmfDOzXrOkCYqQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Zakaria ghrab

ungelesen,
28.11.2016, 04:58:0528.11.16
an material...@googlegroups.com
In that case what'is the  advantage to perform NDE after PWHT.

Thank you.


For more options, visit https://groups.google.com/d/optout.



--

Thanks and Regards, ?

Alan Denney

ungelesen,
28.11.2016, 05:38:4728.11.16
an material...@googlegroups.com

PWHT can open up lack of fusion defects which were held closed prior to PWHT by the residual stresses (and were transparent to UT).

Final acceptance is based on the article in its finished condition. NDT before PWHT is carried out so that repairs on the defects detected at that stage are cleared at that stage.

 

Alan Denney

AKD Materials Consulting Ltd

--

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.



 

--

Dr. Georgios Dilintas,

Dipl. Ing. In Aeronautic and Space Engineering

Ph.D in Mechanics of Solids - Computational Mechanics

A.I.S, A.N.I, IRCA Lead Auditor

Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.



 

--

 

Thanks and Regards, ?

-----

زكرياء غراب
GHRAB Zakaria 

Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB2Z%2B%3DcBXEYsB-r9SBzD3hBZAkHH9Y58oywvET0S2uYOKg%40mail.gmail.com.


For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

George Dilintas

ungelesen,
28.11.2016, 06:28:3528.11.16
an Meghanadh K
residual stresses are usually tensile stresses. This would be the case when residual stresses were compressive ones.

2016-11-28 12:32 GMT+02:00 Alan Denney <al...@denney1.freeserve.co.uk>:

PWHT can open up lack of fusion defects which were held closed prior to PWHT by the residual stresses (and were transparent to UT).

Final acceptance is based on the article in its finished condition. NDT before PWHT is carried out so that repairs on the defects detected at that stage are cleared at that stage.

 

Alan Denney

AKD Materials Consulting Ltd

--

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.



 

--

Dr. Georgios Dilintas,

Dipl. Ing. In Aeronautic and Space Engineering

Ph.D in Mechanics of Solids - Computational Mechanics

A.I.S, A.N.I, IRCA Lead Auditor

Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.



 

--

 

Thanks and Regards, ?

-----

زكرياء غراب
GHRAB Zakaria 

Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001501d24962%24b0599810%24110cc830%24%40denney1.freeserve.co.uk.

For more options, visit https://groups.google.com/d/optout.
Allen antworten
Antwort an Autor
Weiterleiten
0 neue Nachrichten