Dear experts,

Pls could approved piping welder weld fillet structral weld?

Thanks 

venkateswara reddy Desireddy

unread,
Apr 18, 2026, 1:24:38 AM (12 days ago) Apr 18
to material...@googlegroups.com
If code of construction b31.3 then no issue. Generally for structure AWS D1.1 will follow. For this code you have to qualify welder. Both codes are different .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANV5n6hdEWEc%2BMM7c8JUyBQSUeH2OQeKHwE8AYeZnAT5GLp9Tg%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages