Impact test requirement for PED 97/23/EC

1,235 views
Skip to first unread message

Kwangju Moon

unread,
Jan 29, 2015, 10:08:49 PM1/29/15
to material...@googlegroups.com

Dear experts,

Please clarify below questions.

Back Ground:

-       Applicable construction code: ASME Sec. VIII, Div.1

-       Material : SA516-70N (35mm)

-       Equipment’s MDMT: -20

-       The client request that impact testing shall comply with the code of construction and in accordance with PED 97/23/EC Annex 1, Para 7.5.

 

Question 1):

Shall we have to perform the impact test on this material in accordance with PED requirement even impact test is exempted as per UCS-66, ASME Sec. VIII Div.1?

 

Question 2):

When the impact test is required as per PED, should we have to use WPS with applying all supplementary essential requirements for weld joint?

Prakash Gotimukul

unread,
Jan 30, 2015, 11:20:05 PM1/30/15
to material...@googlegroups.com


Rgds
G.Prakash
Independent Consultant, ASME AIS/ISO
Technical Director, Hitek Engg Services, Dubai
 gpraka...@gmail.com.

On Fri, Jan 30, 2015 at 7:08 AM, Kwangju Moon <xum...@gmail.com> wrote:

Dear experts,

Please clarify below questions.

Back Ground:

-       Applicable construction code: ASME Sec. VIII, Div.1

-       Material : SA516-70N (35mm)

-       Equipment’s MDMT: -20

-       The client request that impact testing shall comply with the code of construction and in accordance with PED 97/23/EC Annex 1, Para 7.5.

 

Question 1):

Shall we have to perform the impact test on this material in accordance with PED requirement even impact test is exempted as per UCS-66, ASME Sec. VIII Div.1?

 

YES​ for material.

 

Question 2):

When the impact test is required as per PED, should we have to use WPS with applying all supplementary essential requirements for weld joint?


​Follow ASME code requirement​
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/59ddf4e5-821f-4c9c-b504-95902341d46a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

S.Mohammed

unread,
Apr 28, 2015, 10:10:17 AM4/28/15
to material...@googlegroups.com
Ans1:yes or u can send justification as per ASME.

Ans2: yes if impct conducted then all supplimentry variable applicable.
Reply all
Reply to author
Forward
0 new messages