Dears,
Good day.I have one doubt about LTCS PQR regarding
temperature limit.Our PQR specimen is 5mm thickness and impact test at
2.5mm thick.In your design temp.is -46 degree.In ASME 31.3 and section
viii says .this 2.5 mm specimen allowed for -27degree.But our client comment is this PQR IS used only
-28 degree only.So explain about the correct thickness of specimen for
impact test at -46 temp.design temp.
Thanks and Regards
On Thursday, April 19, 2012 at 8:42:35 AM UTC+3, Darshan Maheshwari wrote:Can any body suggest what thickness range is applied for qualifying a WPS (for thickness 7.11mm) for LTCS piping material. Please provide reference also.Regards,Darshan Maheshwari.