Great to hear from you.

Which filler is required to weld ss Pipe to Pipe  ASTM A554 Type 304.


Thanks, Regards.

 

Battini Simhachalam

QC Inspector – Quality Dept. 

ArRiyadh New Mobility - CWG

6th Floor, ArRiyadh New Mobility Building

Olaya Street (North) – Al Sahafah District

P.O. Box 99816 – Riyadh 11625 – Saudi Arabia

M +966 546044327

simhachal...@cwg-metro.com

www.anm-metro.com

24°46'57.42"N  46°38'26.10"E

Location map (click here)

Simhachalam Battini

unread,
Nov 13, 2022, 10:20:45 PM11/13/22
to Materials & Welding
Dear Experts

Which filler wire is required to weld ss Pipe to Pipe  ASTM A554 Type 304.

Kannayeram Gnanapandithan

unread,
Nov 21, 2022, 1:56:08 AM11/21/22
to material...@googlegroups.com
308
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABk4cbF476CBNYD5%2By1NJAYOZVXZKFNWe0tuiV%2B1SV%2BipuhwMw%40mail.gmail.com.

Simhachalam Battini

unread,
Nov 22, 2022, 5:26:02 AM11/22/22
to material...@googlegroups.com
Dear Expert.
Thank you for your information, 

If we will use 316L filler wire what is the effect for welding?



G Gughan

unread,
Nov 29, 2022, 10:17:19 PM11/29/22
to material...@googlegroups.com

Dear Battini,

When your material is 304, the 308 filler wire is sufficient for strength & integrity.

If 308 meets your materials' chemical composition requirements, why do you want to use 316L?

308 is more economical than 316L. An Essential part is to pass the mechanical test as required/client specifications.

There is no effect if you use 316L. All the obtained results will be higher than your material specs.

Please refer to ASME SEC II Part-C SFA 5.9 for SS filler wire. It will assist you.