Filler wire requirement for A516 Grade 70

29 views
Skip to first unread message

Tajuddin Mohammed

unread,
Oct 26, 2025, 6:16:41 AM10/26/25
to material...@googlegroups.com
Dear experts,

      We have A516 Grade 70 material which is being used in one of our projects. Please kindly advise which  electrode or filler metal to be used as per AWS D1.1
SMAW electrode-?
FCAW filler wire-?
SAW filler wire-?


Thanks & Regards
Mohammed Tajuddin
WELDING INSPECTOR CSWIP 3.1
Contact  0530833486
JUBAIL

venkateswara reddy Desireddy

unread,
Oct 26, 2025, 8:48:34 AM10/26/25
to material...@googlegroups.com
SMAW electrode- E 7018
FCAW filler wire- E71T-1
SAW filler wire- EM12K  Flux-F7A6 

These are commonly used. but if project have any special requirements we have choose other electrode.




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACZrEUap%2B3yKmNp%2BMS6H_CA%2B%3DKpsJULF1pZSTGXJW2VuijJe1Q%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages