P no. & group no. for IS 1079 material
44 views
Skip to first unread message
Brijesh Maurya
unread,
Jul 13, 2020, 8:10:18 AM
7/13/20
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
hello experts,
can anybody clarify, what is the P no. & Group no. for IS 1079 sheet material?
Thanks in advance.....
Rajnish Dixit
unread,
Jul 14, 2020, 6:54:15 AM
7/14/20
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Hi,
This material does not have any P/Group No. as per ASME Section IX. In the space "unassigned" to be written when WPS/PQR will be prepared.
Thanks,
Best Regards,
Rajnish
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com
.