UT or RT for LNG thanks

128 views
Skip to first unread message

Brl Pp

unread,
Dec 5, 2010, 1:01:22 PM12/5/10
to material...@googlegroups.com
Good morning for all,

This preocupation is for LNG thanks (120 000 m3 capacity).

As per the contract and procedure, the radiography test (RT) is
required. My contractor needs to do the ultrasonic test (UT).

My question is:
To do the ultrasonic test (UT) or the radiography test (RT)?

Tanks in advance and have a nice day.


Redouane (Project engineer)
Algeria

manoj vernekar

unread,
Dec 5, 2010, 10:50:18 PM12/5/10
to material...@googlegroups.com
Hi
 
NDT requirements should be  clearly specified in client specification.
Shell requirement is 100% RT and 100% Tee and long seam.
regards
 
manoj

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Manoj.Vernekar

Marcelo P. Soriano Qa/Qc Eng'r.

unread,
Dec 6, 2010, 12:12:47 PM12/6/10
to Materials & Welding
try to check your project specs i am sure that is mention there the
limitation of rt and ut. some points is base in the thickness of
material.

marcelo

On Dec 6, 6:50 am, manoj vernekar <manojverne...@gmail.com> wrote:
> Hi
>
> NDT requirements should be  clearly specified in client specification.
> Shell requirement is 100% RT and 100% Tee and long seam
> regards
>
> manoj
>
>
>
>
>
>
>
>
>
> On Sun, Dec 5, 2010 at 10:01 PM, Brl Pp <refazosa...@gmail.com> wrote:
> > Good morning for all,
>
> > This preocupation is for LNG thanks (120 000 m3 capacity).
>
> > As per the contract and procedure, the radiography test (RT) is
> > required. My contractor needs to do the ultrasonic test (UT).
>
> > My question is:
> > To do the ultrasonic test (UT) or the radiography test (RT)?
>
> > Tanks in advance and have a nice day.
>
> > Redouane (Project engineer)
> > Algeria
>
> > --
> > To post to this group, send email to material...@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-weld...@googlegroups.com<materials-welding%2Bunsu...@googlegroups.com>

pgoswami

unread,
Dec 6, 2010, 10:49:17 PM12/6/10
to material...@googlegroups.com

Hi Redouane,

ASME allows UT in lieu of RT but not as a blanket approval.Under the above code case on a specific case by case basis this change of NDE technique is acceptable. But the UT technique should not be conventional pulse echo type, it has to be state of art digitized UT techniques such as TOFD or Phased Array.

If the design code for the LNG tank is API-620, then the following is the selection criteria of UT in lieu of RT.

7.15.3 Ultrasonic Examination Method

7.15.3.1 Ultrasonic Examination in Lieu of Radiography:-When ultrasonic examination is applied in order to fulfill the requirements of 5.26, Q.7.6, or R.7.6, the provisions of Appendix U shall apply. Appendix U also talks about the NDE techniques mentioned above.


Let me know, if it helps.

Thanks.

Pradip Goswami,P.Eng.,IWE.
Welding & Metallurgical Specialist & Consultant
Email-p...@sympatico.ca,
pgos...@quickclic.net

-----Original Message-----
From: material...@googlegroups.com [
mailto:material...@googlegroups.com] On Behalf Of Marcelo P. Soriano Qa/Qc Eng'r.


> > For more options, visit this group's bolg at
> >

> > The views expressed/exchnaged in this group are members personel
> >views and  meant for educational purposes only, Users must take their
> >own decisions  w.r.t. applicable code/standard/contract documents.
>
> --
> Manoj.Vernekar

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at

Use of Ultrasonic Examination in Lieu of Radiography.pdf

Brl Pp

unread,
Dec 7, 2010, 1:52:53 AM12/7/10
to material...@googlegroups.com
PGOSWAMI,
Good morning,

Thank you for your answer,

Yes, you are right and I agree with you, the appendix U of API 620
code is very clear, but my opinion it is of not tolerated with my
contractor.

Actually my contractor wants to use UT in place RT for the reasons of
cost because UT is not expensive than RT.

Further to your answer I have to communicate the appendix U of the
code API 620 in races of technique one following of course the
contractual clauses.

Please I want a piping cleaning specification for heat exchanger.

PS: I am sorry to put the similar conversations because I am not
qualified in the quality control and during my career I am only
in the management of project. Also sorry about my English because in
Algeria the French language is prime

Thank you PGOSWAMI and have a good day


My best regards
REDOUANE (Engineer of project)
SONATR ACH – Algeria


2010/12/7, pgoswami <pgos...@quickclic.net>:

manoj vernekar

unread,
Dec 7, 2010, 2:24:00 AM12/7/10
to material...@googlegroups.com
Redouane
 
first you have to see the contract, than specification.
 
If at all you are looking for quality job. 100 % RT (combination of fast and low speed film)on all butt weld long seam and C seam. and 100% UT on long seam and Tee joins.
 
UT RTT ,creep wave probe and zone wise and axial probe movement, and you required LNG experience UT technisions.
 
regards
 
manoj


 
On Tue, Dec 7, 2010 at 10:52 AM, Brl Pp <refaz...@gmail.com> wrote:
PGOSWAMI,
Good morning,

Thank you for your answer,

Yes, you are right and I agree with you, the appendix U of API 620
code is very clear, but my opinion it is of not tolerated with my
contractor.

Actually my contractor wants to use UT in place RT for the reasons of
cost because UT is not expensive than RT.

Further to your answer I have to communicate the appendix U of the
code API 620 in races of technique one following of course the
contractual clauses.

Please I want a piping cleaning specification for heat exchanger.

PS: I am sorry to put the similar conversations because I am not
qualified in the quality control and        during my career I am only
in the management of project. Also sorry about my English because in
Algeria the French language is prime

Thank you PGOSWAMI and have a good day


My best regards
c (Engineer of project)



--
Manoj.Vernekar

K K

unread,
Jul 13, 2020, 11:38:54 PM7/13/20
to Materials & Welding
Dear Sir,

According to API 650 Appendix U.

If We will not use the Ultrasonic Examination in Lieu of Radiography. We have sufficient resources to complete the NDT requirement with RT.
Then can we accept the procedure?

Regards 
Kiran

] On Behalf Of Marcelo P. Soriano Qa/Qc Eng'r.


> > For more options, visit this group's bolg at
> >

> > The views expressed/exchnaged in this group are members personel
> >views and  meant for educational purposes only, Users must take their
> >own decisions  w.r.t. applicable code/standard/contract documents.
>
> --
> Manoj.Vernekar

--
To post to this group, send email to material...@googlegroups.com

To unsubscribe from this group, send email to material...@googlegroups.com


For more options, visit this group's bolg at

SENTHILKUMAR SWAMINATHAN

unread,
Jul 14, 2020, 3:07:19 AM7/14/20
to material...@googlegroups.com
Perform RT on the said weld is Acceptable. If you want to do UT, then meet the Appx - U requirement is mandatory. 

Regards, S.SENTHILKUMAR


https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3ae63611-4492-4d12-a28d-68e0fefca63co%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages