I Am working on WPS  and material will be SS 316 L to SS 316 L

My Qus:-

We can use the E316L filler rod for this material, as well as determine the F-number for this consumable.

Thanks.

Parminder Singh

neprebran,
4. mar. 2024, 08:22:484. mar.
do material...@googlegroups.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2410bde9-23ba-423c-9a88-38c1d6397f93n%40googlegroups.com.

Arief Krisnadi

neprebran,
4. mar. 2024, 21:37:304. mar.
do material...@googlegroups.com
Please use google search.
It is very useful and impressive tool in the world. 

image.png



--
Odgovori vsem
Odgovori avtorju
Posreduj
0 novih sporočil