API 2b straightness interpretation

154 views
Skip to first unread message

vikas waghmare

unread,
Jul 28, 2013, 12:40:01 AM7/28/13
to material...@googlegroups.com
Dear All,
 
As per the below clause of API 2B

6.4 STRAIGHTNESS

The maximum allowable straightness deviation in any 10-

ft length shall be

1/8 in. For lengths over 10 ft, the maximum

deviation of the entire length may be computed by the following

formula, not to exceed

3/8 in. in any 40-ft length.

My question is , if we have 40 ft length then we have to consider both the point i.e is any 10 ft it shall be max. 1/8" and total length 3/8" or only the second part.

 

Please advise

 

Regards,

 

Vikas waghmare

krishnaraj koduvally

unread,
Sep 10, 2015, 1:13:56 PM9/10/15
to Materials & Welding
Dear Vikas,

  Hope you have got the clarification. Please share with me i also have the same doubt. rajuth...@gmail.com