Pl share AIR FIN FAN cooler SS316 MOC fabrication sequence to avoid partition plate distortion
Thr partition plate is distorting in its full length after full welding the corner 4nos (32 mm groove )of Square Box Header welds
GTAW + SAW is used

Pl guide

Sent from my iPhone

Nambirajan Avudaiappan

unread,
Apr 25, 2025, 12:11:29 AM4/25/25
to material...@googlegroups.com
Dear vishwas sir, 

Why we can try spider to avoid the distortion correct me if I am wrong. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/2E591BA9-F1C2-4331-8B27-A395AF0477D8%40gmail.com.

Vishwas Keskar

unread,
Apr 25, 2025, 3:49:34 AM4/25/25
to material...@googlegroups.com, material...@googlegroups.com
It is closed square box 
Sent from my iPhone

On 25 Apr 2025, at 9:41 AM, Nambirajan Avudaiappan <nambirajan...@gmail.com> wrote: