Orifice flange root flushing

259 views
Skip to first unread message

tdky167

unread,
Feb 24, 2016, 10:41:20 PM2/24/16
to material...@googlegroups.com
Good morning folks ,

Does code suggest NDE ( MPI or PT ) to be carried out once the root of the orifice flange is flush grinded .



Sent from my Mi phone

Tamil

unread,
Feb 25, 2016, 1:23:18 AM2/25/16
to material...@googlegroups.com
Only surface NDT anything OK
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/q7tpbdl1tpuppkigf21luoj8.1456371624313%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

Pradeep Chowdary

unread,
Mar 10, 2016, 4:47:11 AM3/10/16
to Materials & Welding
Dear Yokesh,

Code doesn't suggest NDE on Orifice Flange. It's depend upon the client, here we face the same issue and we done with PT that too 10% .

If anything lemme know..

Pradeep 