Enquiry about lower shell MPI while replacing Annular Plate in storage tank

34 views
Skip to first unread message

tahir alam

unread,
Jul 9, 2018, 11:29:33 PM7/9/18
to material...@googlegroups.com
Dear experts 

We have contract of tank maintenance in Kuwait. While replacing annular plate inspection ask to do DPT of 2 inch of shell plates. In another refinery they are agree to do MPI only while replacing the annular plates. kindly guide me which one is mention in code. If specifically mention in code then pls send me code detail also.

Best Regards
Tahir Alam
Planning Engineer
Agam Tank Maintenance Group
Mobile : +(965)5150-1509


--------------------------------------------------------------------------------
Site Office : +(965)2388-3614
Head Office : +(965) 2398-5381l2
Fax : +(965) 2398-8312
P.O.Box : 9390 Ahmadi, 61004 Kuwait
Email : tahira...@gmail.com
Website : www.agamltd.com
-------------------------------------------------------------

PGoswami

unread,
Jul 9, 2018, 11:40:22 PM7/9/18
to material...@googlegroups.com

What’s the design code? Is there any additional requirement such as clients’ specifications.

MPI & LPI are often interchangeable for determination of surface defects.

 

Thanks.

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

tahir alam

unread,
Jul 9, 2018, 11:56:10 PM7/9/18
to material...@googlegroups.com
We are following API 653 ,just wanted to know is it mention in code which test is required to check shell surface defect while replacing annular plate. Here two refinery one refinery is accepting MPI and other refinery not accepting MPI ,they told us to do LPT of shell.


Best Regards
Tahir Alam
Planning Engineer
Agam Tank Maintenance Group
Mobile : +(965)5150-1509


--------------------------------------------------------------------------------
Site Office : +(965)2388-3614
Head Office : +(965) 2398-5381l2
Fax : +(965) 2398-8312
P.O.Box : 9390 Ahmadi, 61004 Kuwait
Email : tahira...@gmail.com
Website : www.agamltd.com
-------------------------------------------------------------

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Kishor Swaminathan

unread,
Jul 10, 2018, 1:23:38 AM7/10/18
to material...@googlegroups.com
Hi Dear ,


Annular plate have the inspection for first root DPT ,final UT,  then shell to annular plate diesel chalk test,VBT, outside .MPI OR LPT


REGARDS,

KISHOR
WELDING INSPECTOR 

TARIQ ALGHANIM 

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages