skipping of PWHT (SR) and Hydrotest

60 views
Skip to first unread message

Shahil Saini

unread,
Jan 19, 2022, 1:11:10 AM1/19/22
to material...@googlegroups.com
Hello everyone,

If the weld performed is sound on the 32 mm thik material (SS and CS) and preheated as per code, then can i skip the PWHT and Hydrotest??

Regards,
Shahil Saini
PGET-Welding 

Sankaran Sp

unread,
Jan 19, 2022, 1:33:30 AM1/19/22
to material...@googlegroups.com
Dear friend,

If joint welding of SS+ CS with 32mm thickness - as per ASME sec VIII div 1 for p no :1 PWHT is mandatory.
> if you preheated the CS side as per code? if the HAZ hardness on CS plate is within the base metal range, you can avoid PWHT process if end customer is accepting  this condition 
  

Regards,
Sankaran.SP
Welding & Metallurgy expert
coimbatore, India.  


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-_JBJx8S4Yph3nt%3DoC0e%2BvKMd1RMA_6hfowNBTaGKyEA%40mail.gmail.com.

Dinesh Somwanshi

unread,
Jan 19, 2022, 10:15:36 PM1/19/22
to materials-welding
Dear team,

Anybody knows about 6 yrs renewal Api 570 certification guidance and update.

Pls advise 
Dinesh 9881344135 WhatsApp

Thanks & Regards
Dinesh

Shridev Kurup

unread,
Jan 20, 2022, 12:51:08 AM1/20/22
to material...@googlegroups.com
Please vist your account in Api.org in section individual certification ICP.  Log in with user id and password. Any trouble write to api for new password or login details. 

After 6 years may be online quiz will be required and it may be clearly defined there when you log in.

Complete the quiz and complete all other requirements stipulated and then you will reach to final payment section.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Gopalakrishnan G

unread,
Jan 24, 2022, 11:51:30 PM1/24/22
to material...@googlegroups.com
No you can't skip pwht and hydrotest

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Mohd Siraj

unread,
Feb 8, 2022, 10:18:49 PM2/8/22
to Materials & Welding
you need demonstrate CPD!

just log on to your account, API will guide you, i have received one mail from API recently. in that very detailed instructions are given on how to proceed...

Reply all
Reply to author
Forward
0 new messages