You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
I need a recommendation for suitable paint specification of internal painting (bottom plate & shell course) of petroleum refinery intermediate product tank with steam coil.
Due to temperature epoxy or polyurethane paint spec may not last.
Rupam Manna
unread,
Aug 18, 2022, 4:46:52 AM8/18/22
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Dear Team
Which electrode I have to use for disimiler E355 & 316 material