A 516 GR 70 material welding

58 views
Skip to first unread message

topal...@gmail.com

unread,
Feb 9, 2023, 5:28:15 AMFeb 9
to Materials & Welding

A 516 GR 70 Does the material require heating after welding?(we are welding at 0 degree in Ammonia Tank project)

Babur Khan

unread,
Feb 19, 2023, 9:59:55 PMFeb 19
to material...@googlegroups.com
Greetings,
Please share Construction Code, material (A516) thickness and service temperature. 

Muhammad Babur Khan
Sent from my iPhone

On 9 Feb 2023, at 3:28 PM, topal...@gmail.com <topal...@gmail.com> wrote:



A 516 GR 70 Does the material require heating after welding?(we are welding at 0 degree in Ammonia Tank project)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/05790807-4af8-49ca-bddd-2a3589c59479n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages