Please clarify as per which code we can make the PWPS for SS water bar.

And Unlisted material like EN10025- 2 S 235 JR- how i can get the P.No. and which electrode shall i use for SMAW process.

Regards
K K

MAGHROUD Moussa

unread,
May 21, 2019, 5:34:12 AM5/21/19
to material...@googlegroups.com
1. PSWP as per ISO 15614
2. For S235 JR is CS, P N1, check chimic and mecanic analysis.  


Envoyé depuis mon smartphone Samsung Galaxy.

-------- Message d'origine --------
De : K K <kara...@gmail.com>
Date : 15/05/2019 12:54 (GMT+01:00)
À : Materials & Welding <material...@googlegroups.com>
Objet : [MW:29588] Query for Code and S 235JR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33988233-1a3a-4eb9-a0e5-a0e8c782a372%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

George Dilintas

unread,
May 22, 2019, 5:10:13 AM5/22/19
to material...@googlegroups.com
235JR is P-No 1 because it is  listed in QW/QB-422 and not because of the chemical composition



For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages