Time lag between Hydro test Dewatering completion and swabbing completion

27 views
Skip to first unread message

pradip kumar Sil

unread,
Dec 2, 2019, 4:24:33 AM12/2/19
to materials-welding
Dear All,
Can anybody inform me How much  time lag between Hydro test Dewatering completion and swabbing completion in the pipeline with code reference.
Regards
Pradip

Noufal Mc

unread,
Dec 2, 2019, 11:05:34 PM12/2/19
to material...@googlegroups.com
Pradip,

As per ADNOC specification De watering should be completed within one week. please see below snapshot extracted from DGS 9550-002 rev 1.


image.png
regards 

NOUFAL MC

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DdXk%2BFh7JXe-062dsyd6c0_2%2BSGaSusbbgGPyBPFymcA%40mail.gmail.com.

pradip kumar Sil

unread,
Dec 3, 2019, 1:18:03 AM12/3/19
to materials-welding
Thanks for your update.
My concern is time lag between Dewatering to swabbing activity

Shashank Vagal

unread,
Dec 5, 2019, 1:21:33 AM12/5/19
to material...@googlegroups.com
Immediately after dewatering

Best Regards,

Shashank C Vagal (+91) 8082395502, 8779046302,

301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA