Different between E8018-b2 / E8018

312 views
Skip to first unread message

Hari krishna

unread,
Jul 18, 2022, 7:43:00 AM7/18/22
to Materials & Welding
Dear sir

what is the difference between E8018-b2 / E8018, where there will be major differences or minor? 

when will this difference be seen seriously?

Thanks All :)


Dinesh Somwanshi

unread,
Jul 18, 2022, 11:22:43 PM7/18/22
to materials-welding
Dear sir,

Chrome % is varies.

Thanks 
dinesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/412ec4ee-f360-49a3-a610-6b7019baceb6n%40googlegroups.com.


--
Thanks & Regards

Engr. Dinesh Vitthal Somwanshi

API 510 - Pressure vessel Inspector
API 570 - Piping Inspector, 
AWS - CWI, CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
 00919881344135 India 
Skype = Dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

Sham Shahabuddin -Welding Inspector, HANBO

unread,
Jul 18, 2022, 11:22:44 PM7/18/22
to material...@googlegroups.com
Dear Hari

E 8018-B2 is a low alloy CS Electrode. B2 in this represents the alloy content in the electrode. Please refer ASME SEC II C PART- SFA 5.5 for details of various electrodes in the low alloy CS. As per my knowledge E8018 is not mentioned in the standard which means this electrode is not available. 

Regards
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING
HANBO ENGINEERING & CONSTRUCTION
MARJAN INCREMENT PROGRAM ( MIP - PKG 6 )


Kannayeram Gnanapandithan

unread,
Jul 20, 2022, 2:09:40 AM7/20/22
to materials-welding
B2 is a chrome moli steel. 1.25 Cr, 0.5 Mo
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


binit kumar

unread,
Jul 27, 2022, 12:55:21 AM7/27/22
to material...@googlegroups.com
Dear Mr. Hari,

Thank you for your question.
 I am totally agreed with Mr. sham reply.

Regards,
Binit Kumar(Welding Inspector)
Doosan Power Projects Pvt. Ltd.
NTPC Barh, Bihar

On Mon, Jul 18, 2022 at 5:12 PM Hari krishna <autocads...@gmail.com> wrote:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/412ec4ee-f360-49a3-a610-6b7019baceb6n%40googlegroups.com.


--
BINIT KUMAR
+918717929495
Reply all
Reply to author
Forward
0 new messages