what is the permissible Long Seam Welding orientation closest distance for ERW pipe to pipe welding.

1,137 views
Skip to first unread message

Durgesh

unread,
Jan 15, 2020, 6:20:18 AM1/15/20
to Materials & Welding
please refer attached sketch for better understanding.,

Pleas suggest permissible welding procedure with reference ASME standard. 
forum.pdf

Rishikesh Kumar

unread,
Jan 15, 2020, 10:33:44 PM1/15/20
to material...@googlegroups.com
it is recommended to use the long seam weld shall be 90 to 180 degree orientation between two pipes. it helps to restrict crack  propagation during failure. 

On Wed, Jan 15, 2020 at 4:50 PM Durgesh <durgesh...@galiakotwala.in> wrote:
please refer attached sketch for better understanding.,

Pleas suggest permissible welding procedure with reference ASME standard. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e8c953fc-6602-4c81-9ccc-329d270235a7%40googlegroups.com.

nguyen tuan

unread,
Jan 16, 2020, 6:04:29 AM1/16/20
to material...@googlegroups.com
Pls. find attached file.

Vào Th 5, 16 thg 1, 2020 vào lúc 10:33 Rishikesh Kumar
<rish...@gmail.com> đã viết:
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXs1KqXmuT6u6a7SJ_dES2LPX9j7i9mxpN%3DBy%3Db7n9bu1j39w%40mail.gmail.com.
twi-global.com-What are the standard requirements on the proximity of welds.pdf

Dindo

unread,
Jan 16, 2020, 10:17:29 PM1/16/20
to material...@googlegroups.com
ASME Section VIII Div.1 2017 Edition UW-8(d): Except when longitudinal joints are radiographed 4 in. (100mm) each side of each circumferentialo welded intersection, vessels made up of two or more courses shall have the centers of the welded longitudinal joints of adjacent courses staggered or separated by a distance of at least 5 times the thickness of the thicker plate.