Dear Expert,

“X” welder working with company and left the organization. Again after Two or three year he is joining back same company. All earlier certificate is available with company with proper documentation.

 

Is it possible to renew his earlier certificate with one sample based on RT or visual inspection OR All new qualification is to be done New. Qualification code is ASME SEC IX.

 

Pls provide your valuable input with standard reference.

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar

moksh...@yahoo.co.in

unread,
Dec 27, 2015, 11:30:39 PM12/27/15
to material...@googlegroups.com
Welder X should go for Re qualification because he left the company and he Re joined after 3 years and a welder qualification is required if he didn't welded any joint for 6 month in the same location or same company.

Sent from my ASUS
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXSMVhvN0Fje56BbuQb6V3KSYO%3Dz17%2BLtshZO1u3Vt%2Bkhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
Dec 27, 2015, 11:30:40 PM12/27/15
to Mohd Azam
He has to be qualified again since he has stopped working for a period longer than 6 months

Sent from my BlackBerry 10 smartphone.
From: Mohd Azam
Sent: Κυριακή, 27 Δεκεμβρίου 2015 - 16:32
Subject: [MW:24008] Welder Qualification as per ASME SEC IX
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXSMVhvN0Fje56BbuQb6V3KSYO%3Dz17%2BLtshZO1u3Vt%2Bkhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Dinesh Somwanshi

unread,
Dec 27, 2015, 11:30:40 PM12/27/15
to materials-welding

Dear you can check his continue progress record of earlier based on that will able to test with RT or bend test.

--

james gerald

unread,
Dec 27, 2015, 11:36:06 PM12/27/15
to material...@googlegroups.com
Dear Azam,

Welder Qualification shall be performed by each Qualifying Organisation according to ASME Sec.IX.

Yes the previous Qualification made by the X welder before leaving the organisation will be valid by qualifying a single test coupon for that process.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677




From: Mohd Azam <azam...@gmail.com>
To: material...@googlegroups.com
Sent: Sunday, December 27, 2015 5:48 PM

Subject: [MW:24008] Welder Qualification as per ASME SEC IX
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

Bharat Kumar

unread,
Jan 1, 2016, 1:20:59 PM1/1/16
to material...@googlegroups.com
Hi,

Can that welder be checked for any documentation for the similar works after he left the organisation. I mean that welder might have been working in different organisation but what if he/she had been working with the same welding parameters (this is just to say about his consistency in welding) and these documents are available?

Can that welder be waived off to re-qualify based on these documents as this will prove his consistency. 




For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards,

A Bharat Kumar

george....@gr.bureauveritas.com

unread,
Jan 1, 2016, 7:04:35 PM1/1/16
to Bharat Kumar
No way

Sent from my BlackBerry 10 smartphone.
From: Bharat Kumar
Sent: Παρασκευή, 1 Ιανουαρίου 2016 - 20:21
Subject: Re: [MW:24028] Welder Qualification as per ASME SEC IX


For more options, visit https://groups.google.com/d/optout.

Kannayeram Gnanapandithan

unread,
Jan 2, 2016, 12:06:26 AM1/2/16
to materials-welding

Get continuity records of welding carried out for that process and based on continuity u can extend his validity.

Rajagopal Kannan

unread,
Jan 4, 2016, 4:38:12 AM1/4/16
to material...@googlegroups.com
Hi Bharta kumar,
No. He has to qualify in your quality system.
Thanks and Best Regards,
K.Rajagopal

pgoswami

unread,
Jan 4, 2016, 7:02:13 AM1/4/16
to material...@googlegroups.com

Hi Mohd. Azam,

 

Please look though the following extracts from Sec-IX. It’s advisable to test and qualify the welders separately  and before assigning them in production joints.

 

Thanks..

 

Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

All provided answer are personal opinions or personal judgements only. It's not connected with any employers by any means. 

 

QG-106.3 Simultaneous Performance Qualifications.

 

(f) When the person changes employers between participating organizations, the employing organization shall verify the continuity of the persons qualifications has been maintained by previous employers since his qualification date, as required by the applicable Part for the joining method. Evidence of activities supporting performance qualification continuity may be obtained from any member of the association, even if the member was not a participant in the simultaneous welder qualifications.

 

(g) If a person has had their performance qualification withdrawn for specific reasons, the employing organization shall notify all other participating organizations that the persons qualification(s) has been revoked. The remaining participating organizations shall determine whether or not they will uphold or withdraw the performance qualifications for that person in accordance with this Section.

 

(h) When a persons performance qualifications are renewed in accordance with the provisions of the applicable Part for the joining method, the testing procedures shall follow the rules of this paragraph. Each renewing organization shall be represented by an employee with designated responsibility for performance qualification.

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Rajagopal Kannan


Sent: Sunday, January 03, 2016 11:45 PM
To: material...@googlegroups.com

Tom Kucera

unread,
Mar 1, 2016, 11:25:39 PM3/1/16
to Materials & Welding
What about QG 106.3 ?

Agustin Jimenez

unread,
Mar 2, 2016, 6:19:24 AM3/2/16
to material...@googlegroups.com
Hi.
Whats Standard are you using in project?
Is posible with visual and rt only but There are case where mechanical test is required.

Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: Tom Kucera <tfku...@gmail.com>
Fecha:01/03/2016 04:01 PM (GMT-04:30)
Para: Materials & Welding <material...@googlegroups.com>
Cc:
Asunto: [MW:24422] Re: Welder Qualification as per ASME SEC IX
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

santosh sharma

unread,
Mar 2, 2016, 10:38:59 PM3/2/16
to material...@googlegroups.com

Suppose welder leave the co.and again join  mid gap 6 month requalified of welder

Kannayeram Gnanapandithan

unread,
Mar 3, 2016, 1:15:37 AM3/3/16
to materials-welding
If welder has proof of working in other company and certified by them , u can extend his qualification by any position, material welding with Xray

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

Naskabir Vengassery

unread,
Mar 4, 2016, 1:57:31 AM3/4/16
to Materials & Welding
Dear Azam,
in my opinion considering only ASME Sec IX,
1) if you are confident on the Welder's skill , you can take advantage of ASME Sec IX:2013, QW-322.2 by arranging a test using each processes that he was previously qualified. only process is important. material, shape, thickness, positions and electrical or other parameters are not restricted. After visual you can go for RT in lieu of Bend test. This will revalidate all his previous qualification with the same PROCESS(s).
2) if the welders ability is under doubt or he was not successful in (1) above, retests for all his previous qualifications has to be carried out (QW-322.2(b))

anosh wankhade

unread,
Mar 5, 2016, 1:24:43 AM3/5/16
to material...@googlegroups.com
Dear Mr. Mohd. Azam,

please refer QW 322.1 for expiration of qualification and 322.2 for renewal of qualification.
For your case qualification has expired as per 322.1(a) and re qualification should be done as per 322.2 (a).

Regards,

Anosh Wankhade

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >
Reply all
Reply to author
Forward
0 new messages