Hi Alll can anyone explain me what is meant by oscillation in welding.
is it related to weaving

Phil...@esab.net

unread,
Jun 8, 2010, 3:14:03 AM6/8/10
to materials-welding
Yes oscillation is the same as weaving and the width of the weave should be determined by electrode size and heat input allowable

Best Regards

PHIL CHEW

Global Segment Manager -Transport ,Shipbuilding,M&R

ESAB Holdings Ltd, 322 High Holborn, London, UK, WC1V 7PB

Tel: +44 (0) 7584 219132

email: PHIL...@esab.net

ESAB Holdings Ltd is a company registered in England and Wales . Co registration no 1687590 Registered Office: 322 High Holborn, London , UK , WC1V 7PB www.esab.comPlease consider the environment before printing this email.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________
This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it.

ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

pankaj abhang

unread,
Jun 9, 2010, 1:26:24 AM6/9/10
to material...@googlegroups.com
Dear Mr. Phil I want to know what it means " weaving should not be more than 2-3 times the electode dia.
 
 
 
Pankaj

george....@gr.bureauveritas.com

unread,
Jun 9, 2010, 4:41:01 AM6/9/10
to material...@googlegroups.com

No fellows, oscillation is not the same as weaving.
Please have a look on ASME BPVC section IX - QW-410. 1 for string/weave in SMAW and GMAW and QW-410.7 for oscillation in GTAW and SAW

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for Phil.Chew@esab.netPhil...@esab.net



To

"materials-welding" <material...@googlegroups.com>

cc


Subject

Re: [MW:5457] oscillation and weaving

Ref

Reply all
Reply to author
Forward
0 new messages