IP Joint

71 views
Skip to first unread message

Saurabh Jain

unread,
May 24, 2025, 10:48:32 PM5/24/25
to material...@googlegroups.com
Hello experts,

I would like to know what is IP joints in piping(31.3)? 

Regards
Saurabh

Eugene Matsko

unread,
May 25, 2025, 10:00:39 PM5/25/25
to material...@googlegroups.com
In essence, an IP pipe joint is any connection made between pipes that are sized using the IPS or NPS standards, regardless of the specific connection method.

Sent from my iPhone

On May 24, 2025, at 9:48 PM, Saurabh Jain <ensa...@gmail.com> wrote:


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL_mAcbc5GDt1TSd_Oip4ns3sqL_mS_AOtP4PyW7a9V9OQ%40mail.gmail.com.

George Dilintas

unread,
May 26, 2025, 4:26:46 AM5/26/25
to material...@googlegroups.com
Are you sure? There is no such a term in 31.3
Δρ. Γεώργιος Διλιντάς
Ηπείρου 5 , Μελίσσια - 15127
Αεροναυπηγος Μηχανικός - Μελος ΤΕΕ 55018
Τηλ +30 210 8100578, +30 6944 646 204

Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I,  Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis


Ganga Prasad

unread,
May 26, 2025, 12:27:53 PM5/26/25
to material...@googlegroups.com
Greetings,

I think 'IP' joint means 'incomplete penetration'(partial penetration) joint.




Dhanabal Jalachandran

unread,
May 26, 2025, 2:28:16 PM5/26/25
to material...@googlegroups.com
Greetings,

In Saudi Aramco projects, the term "IP" refers to the Initial Production weld for piping joints. As per the requirements of SAEP-324 (Welder Performance Qualification Procedure), every welder must perform a minimum of three (3) Initial Production (IP) welds following the successful completion of their Welder Qualification Test (WQT).

This process ensures that welders not only meet qualification standards in a controlled test environment but also demonstrate their proficiency in actual site conditions before being released for production welding activities.  

Reference - SAEP-324

Best Regards
Dhana

Saurabh Jain

unread,
May 27, 2025, 12:32:29 AM5/27/25
to material...@googlegroups.com
Many thanks Dhana. 

I am new to Aramco project. I will go through the specs. 

Regards 
Saurabh