In imergency can we get welding done, skipping lamination examination by ut? can it be cover up by complete ut examination after welding?

Please let me know.

Thanks and regards,

Anand

CHINTUKUMAR GANDHI

unread,
Apr 2, 2023, 6:59:44 AMApr 2
to material...@googlegroups.com
Dear Mr. Anand,

You can do it but it is advisable as a good engg. practice to get the UT done before welding to ensure free from cracks, lamination or segregations.

Thanks & regards,


C. R. GANDHI

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHh2n5MEUcY3GwwW1nBcyhg4sfQa2%3DEprW%3D9Wa40Nzam0tvzJw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages