welding position for Groove Weld in T-Joint

114 views
Skip to first unread message

Devin

unread,
May 2, 2017, 9:42:38 AM5/2/17
to Materials & Welding
Dear Experts,
 
 Please kindly see the joint detail attached below. I got puzzled that what welding position it is in red arrow indicates.
 Previously,I thought it must be Over head position, and Now my fellow tell me it should be Horizontal position.  

  1.  I just checked AWS and ASME code,Note 3 said that  "the angle of rotation of the face is determined by a line perpendicular to the theoretical face of the weld which passes through the axis of the weld.". What the “ theoretical face of the weld” exactly means? Is that means“weld face”?if yes,then the angle become 0 degree for the weld mentioned previously,and welding position fall into Horizontal. 
  2. Please kindly put your comments related to this. Really appreciate it!





Raghuram Bathula

unread,
May 3, 2017, 12:55:21 AM5/3/17
to Materials-Welding
it's horizontal (overhead is considered when weld metal deposited from underneath)
Welding positions given in the figures are always contiguous. 
e.g. inclination of the axis between 0° to 15° fall in for both horizontal and overhead.

Chandra

unread,
May 4, 2017, 2:49:57 AM5/4/17
to material...@googlegroups.com
Dear Devin,

Its Horizontal position.

Best Regards,
Chandra
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c4b881c-3468-42fa-ad7a-61362ec46d77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages