Kindly find attached photo of dish end

Seam start & Seam end location I found crack during spinning which is approx 30 mm deep 

Material Sa516 gr 70 
Thickness 50 mm
Weld process SMAW + SAW using E7018-1 & EM12K wire 
IMG-20200216-WA0008.jpg
IMG-20200216-WA0010.jpg
IMG-20200216-WA0011.jpg
IMG-20200216-WA0009.jpg

Charles Jacob

unread,
Feb 18, 2020, 8:43:19 PM2/18/20
to material...@googlegroups.com
Dear,

The photograph shows clear slag entrapped inside and on the sides. Polish the specimen to get a clear picture. Check out your voltage, and travel speed.  Those are the areas of improvement.  

In case of any help contact me. 

Regards, 

Charles V Jacob 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS42HBY7MKhtCozepSdjribf7bU7smX0sWs_Aok85P%3DLcPQ%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages