Require electrode / filler wire details for CR weld overlay on CS with SS 316L

40 views
Skip to first unread message

Mohammed Chand

unread,
Apr 27, 2015, 6:48:25 AM4/27/15
to material...@googlegroups.com
Dear Experts,

I would like to ask what type of electrode or filler wire need to be use for Corrosion resistance weld overlay on CS (P1 Gr 1 material) with SS 316L for SMAW, GTAW and GMAW processes.
And also which type of welding process will be suitable for Flange face weld overlay with SS 316L.
Your kind support in this regards is anticipated.


Thanks and Regards,
Mohammed Chand.

S.Mohammed

unread,
Apr 27, 2015, 11:44:14 PM4/27/15
to material...@googlegroups.com
fisrt layer ER 309 and second layer ER 316L.

surya desai

unread,
Apr 29, 2015, 2:04:03 AM4/29/15
to material...@googlegroups.com
Better u can apply ER 309LMo and Second Layer ER 316L.

Regards
Suryakant

On Mon, Apr 27, 2015 at 7:13 PM, S.Mohammed <mohd...@gmail.com> wrote:
fisrt layer  ER 309 and second layer ER 316L.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5fe586ae-70bf-437f-bb56-a816b42442f8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages