Welding Process for Rail Material A75 ( DIN 536)

182 views
Skip to first unread message

Vinu Raveendran

unread,
Jun 24, 2022, 6:31:50 AM6/24/22
to material...@googlegroups.com
Dear Experts,

Please advise what welding process is recommended to join rail material A75 (DIN 356) and as per which reference code/standard. Also mention what NDT to be performed.

--
VINU RAVEENDRAN

srinivas rao

unread,
Jun 26, 2022, 2:23:47 AM6/26/22
to Materials & Welding

Dear Vinu,
Most commonly used welding process's for  rail welding is 
1. Flash butt welding process  
2. Thermit welding process 

Regards,
Srinivasarao
Welding engineer , GPS 

Sreejith S Nair

unread,
Jun 26, 2022, 9:57:48 AM6/26/22
to material...@googlegroups.com

 Dear Vinu 
 Refer to AWS D15.12 for the Thermite welding process used for rail welding.
 
 
SREEJITH.S NAIR
 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB5wsj%2BkNhp%2Bas4KybezgwRstLbGpJhpA8AyUCEaHNa0MeF3ew%40mail.gmail.com.

vinu raveendran

unread,
Jun 26, 2022, 9:57:52 AM6/26/22
to Materials & Welding
Dear Rao,
Thanks for the advise.

Can you please share as per which code we need to do a PQR coupon  and what mechanical/ NDT tests need to perform for qualifying WPS. 

srinivas rao

unread,
Jun 27, 2022, 11:16:55 PM6/27/22
to Materials & Welding
Dear Vinu ,  
please  refe tthe AWS standard / ISO standrds for this  flash but welding / thermit welding of rails  

AWS D15.2/D15.2M- Recommended Practices for the Welding of Rails and Related Rail Components for Use by Rail Vehicles to get some basic idea about qualification  and ask your cleint are they having project specifcations for  rail welding.
type of tests required for any welding procedure will be confimed by welding code , contrsctuintion code& project specifications& recommended practices applicable for a project .

common test fro rail welds are 
NDT - RT/ UT(PREFERABLE) , MT
weld chemistry 
macro
hardness
metallurgucal test
bend test 
TRANSFER TESTS  
 MICRO (METALLURGYCIAL ANALYSIS )

Thanks & regards, 
Srinivas Rao