Structural WPS as per IS 7307

127 views
Skip to first unread message

Akshith

unread,
Jan 29, 2015, 5:05:30 AM1/29/15
to material...@googlegroups.com
Dear Experts,

Kindly suggest for preparation of structural WPS as per IS 7307, my structural steel thickness range is 4.7mm to 40 mm.
Please suggest thickness range and positions are to be qualified as per IS 7307 & IS 7310.


Regards,

Akshith.

Kunal Patel

unread,
Jan 29, 2015, 12:28:19 PM1/29/15
to material...@googlegroups.com
You have to prepare two WPS for thicknesss of 10 mm and 20 mm. it will be ccover your required thickness range. 
Position can be taken depend upon mfg. or drawing requirement.
Reply all
Reply to author
Forward