http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/539457555.1002882.1476094177885%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

On Thu, 13 Oct, 2016 at 17:16, Prakash Gotimukul<gprak...@gmail.com> wrote:
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qJdz%3DAZaZaj89cNkRRFc0VvbhDqYPq6VWbiBm-YSMUNrQ%40mail.gmail.com.
<20161014_121208.jpg>
Dear Experts
<20161009_132033.jpg>
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1412316375.105633.1476419139756%40mail.yahoo.com.
<20161014_121208.jpg>
<20161009_132033.jpg>
Hi,
That EE - sour service with SS internal parts.
NL - No Limit of H2S Concentration.
Thanks and Regards,
Rajagopal Kannan
Dear raj,Can you please specify where is given N and L value in API and what is the component are you looking for?
Sent from my iPhone
On Oct 14, 2016, at 8:25 AM, 'raj susi' via Materials & Welding <materials-welding@googlegroups.com> wrote:
<20161014_121208.jpg>Dear PrakashThanks for your reply.My question here is the -when the design parameter is -20 deg F to 250 deg F, can the Material class be only -50 deg F to 180 deg F?-50 deg F is more than -20 deg F, FINE for minus degree service.But 180 deg F is less than 250 deg F, should the material temperature be equal or greater than Design? this is my question in the previously attached report.regardsraj
On Thu, 13 Oct, 2016 at 17:16, Prakash Gotimukul<gprak...@gmail.com> wrote:
Who gave the design parameters? If given by client then, design it to that. Not the service parameters.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qJdz%3DAZaZaj89cNkRRFc0VvbhDqYPq6VWbiBm-YSMUNrQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1412316375.105633.1476419139756%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
<20161014_121208.jpg><20161009_132033.jpg>--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/EB1F009E-D0DB-4B35-B836-36B390C807E6%40gmail.com.