For your applications:
1. Polysoude P6 + MU IV Open Head + Cold Wire—Suitable for SS 25 NB to 300 NB and 2–10 mm wall thickness.
2. AXXAIR SAXX 300 + Open Head—An alternative with a user-friendly interface.
Both brands are available in the commercial market and may cost between 20 and 50 lakhs, depending on the
configuration.
Your 10 mm thick and 300 NB size requires an open-head or carriage-type orbital system with a wire feed.
A closed head is ideal for thin-wall tubing.
Equipment Configuration should have:
Inverter orbital power source
Open orbital welding head
AVC (Arc Voltage Control)
Torch oscillation
Cold wire feeder
Water cooling
Weld data logger
Oxygen analyser (for purge monitoring)
Internal pipe purging system
Remote pendant
Weld procedure memory (at least 200 to 300 programs)
Both systems are good for dairy, pharma, food processing, and SS fabrication. If you have any other brand in
mind, please go ahead.
C Sridhar.
------------------------------------------------------------------------------------------------------------------------------------------------
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/5a3bf8d7-b258-4a6e-aa65-678704845196n%40googlegroups.com.
Lincoln Electric – STT mechanised pipeline systems.
Fronius – CMT mechanised pipeline systems.
CRC-Evans – Integrated automatic pipeline welding systems.
Serimax – Premium offshore pipeline welding systems.
are generally recommended.
These companies work through project-based sales and engineering support rather than stocking equipment
through conventional dealers.
C Sridhar.