Gentlemen,

Can anyone suggest a suitable best quality automated / orbital welding machine for welding Pipeline girth Welds.
Requirements are.....
* Carbon Steel, Sour Service
* both offshore and onshore works
* open root with STT/CMT preferred

Thankyou

Regards
Suresh 






siril kumar

unread,
Jul 27, 2026, 8:58:07 AMJul 27
to Materials & Welding
Hello Everyone,

Can you suggest any automatic/ orbita welding machines that is suitable for SS304L/ SS316L from thickness of 2mm to 10mm and Pipes from 25 NB to 300 NB.

Regards,

S Kumar

sridhar cn

unread,
Jul 28, 2026, 12:40:51 AMJul 28
to material...@googlegroups.com
Dear Mr Kumar,

For your applications:

1. Polysoude P6 + MU IV Open Head + Cold Wire—Suitable for SS 25 NB to 300 NB and 2–10 mm wall thickness.

2. AXXAIR SAXX 300 + Open Head—An alternative with a user-friendly interface.

Both brands are available in the commercial market and may cost between 20 and 50 lakhs, depending on the 

configuration.


Your 10 mm thick and 300 NB size requires an open-head or carriage-type orbital system with a wire feed.  

A closed head is ideal for thin-wall tubing.


Equipment Configuration should have:

Inverter orbital power source

Open orbital welding head

AVC (Arc Voltage Control)

Torch oscillation

Cold wire feeder

Water cooling

Weld data logger

Oxygen analyser (for purge monitoring)

Internal pipe purging system

Remote pendant

Weld procedure memory (at least 200 to 300 programs)


Both systems are good for dairy, pharma, food processing, and SS fabrication. If you have any other brand in 

mind, please go ahead.


C Sridhar.

------------------------------------------------------------------------------------------------------------------------------------------------






--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/5a3bf8d7-b258-4a6e-aa65-678704845196n%40googlegroups.com.

Aniket Shingewad

unread,
Jul 28, 2026, 5:59:59 AMJul 28
to material...@googlegroups.com
Sir,
You can opt for  closed welding heads from Universal Orbital Systems, Pune.
Considering TIG welding as your application.

Regards,
Aniket


sridhar cn

unread,
Jul 28, 2026, 11:55:36 PMJul 28
to material...@googlegroups.com
Dear Mr. Suresh,

For Pipeline Girth Welding,

Lincoln Electric – STT mechanised pipeline systems.

Fronius – CMT mechanised pipeline systems.

CRC-Evans – Integrated automatic pipeline welding systems.

Serimax – Premium offshore pipeline welding systems.

are generally recommended.

These companies work through project-based sales and engineering support rather than stocking equipment 

through conventional dealers.  

C Sridhar. 

Ashishranjan - Domech Fabricators Pvt.Ltd.

unread,
Aug 12, 2026, 6:48:15 AMAug 12
to material...@googlegroups.com
Programmable orbital GTAW power source, minimum ~300–400 A, pulsed TIG, AVC, oscillation, programmable multi-level sequences, cold-wire feeder, water-cooled orbital heads, data logging, purge-gas control, and interchangeable heads covering approximately 34–324 mm OD.


Regards,

Ashish Ranjan

Go green logo

Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.

"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.

Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."


Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe.



On Mon, Jul 27, 2026 at 6:27 PM siril kumar <siril...@gmail.com> wrote:

Ashishranjan - Domech Fabricators Pvt.Ltd.

unread,
Aug 12, 2026, 6:48:15 AMAug 12
to material...@googlegroups.com

PolysoudeP4/P6 family + appropriate open/carriage headsExcellentExcellent⭐⭐⭐⭐⭐
OrbitalumOrbital TIG power source + HX/pipe headsVery goodExcellent⭐⭐⭐⭐⭐
AXXAIROrbital TIG systems + open headsVery goodVery good⭐⭐⭐⭐½
AMIModel 207/415-type orbital systems + suitable headsVery goodExcellent⭐⭐⭐⭐½

Regards,

Ashish Ranjan

Go green logo

Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.



"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.

Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."


Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe.


Reply all
Reply to author
Forward
0 new messages