electrode selection

269 views
Skip to first unread message

QA/QC Deptt. TCPL

unread,
Oct 28, 2020, 3:55:16 AM10/28/20
to Materials & Welding
Please suggest electrode for welding sa516 & sa105

Jamie Reyes

unread,
Oct 29, 2020, 1:40:45 AM10/29/20
to material...@googlegroups.com
In order to receive the results you are seeking, you should elaborate a bit more. For instance, the type of welding process to be used, service application, service temperature, if impacts are needed, hardness is of concern, etc. If you would like me to just name you any electrode without knowing any of the above mentioned information, I suppose one can recommend for instance, E71T-1 for the FCAW Process, E70C-6M for the MCAW Process, ER70S-2(or -3;-6)for the GTAW or GMAW Process, E7018 for the SMAW Process, just to name a few. Like I stated in the beginning, I suggest specifying what exactly it is that you are seeking to accomplish. Some of the electrode variables can change (designators) in order to meet certain criteria’s, this is why you need to specify more information. Cheers.....

On Wed, Oct 28, 2020 at 12:55 AM QA/QC Deptt. TCPL <q...@tirupatisteel.com> wrote:
Please suggest electrode for welding sa516 & sa105

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96696980-d46c-4c18-a805-f06946c71e3en%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

Vinoth Rajendran

unread,
Oct 29, 2020, 1:40:46 AM10/29/20
to material...@googlegroups.com
E 7018 for SMAW
ER 70S-2 for TIG

On Wed, Oct 28, 2020, 13:25 QA/QC Deptt. TCPL <q...@tirupatisteel.com> wrote:
Please suggest electrode for welding sa516 & sa105

--

Sandeep Pr

unread,
Oct 29, 2020, 1:40:46 AM10/29/20
to material...@googlegroups.com
welding process please..


With Regards,

Sandeep.P.Raghavan


On Wed, Oct 28, 2020 at 11:55 AM QA/QC Deptt. TCPL <q...@tirupatisteel.com> wrote:
Please suggest electrode for welding sa516 & sa105

--

Kishor Swaminathan

unread,
Oct 29, 2020, 1:40:46 AM10/29/20
to material...@googlegroups.com
tirupatisteel 

SA 516 =  E7018
SA 105 = E6010 + E7018


Regards,

Kishor 
qc inspector 

On Wed, Oct 28, 2020 at 10:55 AM QA/QC Deptt. TCPL <q...@tirupatisteel.com> wrote:
Please suggest electrode for welding sa516 & sa105

--

George Dilintas

unread,
Oct 29, 2020, 1:40:54 AM10/29/20
to material...@googlegroups.com
Basically E7018

Στις Τετ, 28 Οκτ 2020 στις 9:55 π.μ., ο/η QA/QC Deptt. TCPL <q...@tirupatisteel.com> έγραψε:
Please suggest electrode for welding sa516 & sa105

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96696980-d46c-4c18-a805-f06946c71e3en%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Emilio Cerato

unread,
Oct 29, 2020, 1:40:55 AM10/29/20
to material...@googlegroups.com
You can use E7018-1


From: material...@googlegroups.com <material...@googlegroups.com> on behalf of QA/QC Deptt. TCPL <q...@tirupatisteel.com>
Sent: Wednesday, October 28, 2020 4:50:10 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:31632] electrode selection
 
Please suggest electrode for welding sa516 & sa105

--

Ankur Pandey

unread,
Oct 29, 2020, 1:40:55 AM10/29/20
to material...@googlegroups.com
E7018

On Wed, Oct 28, 2020 at 3:55 AM QA/QC Deptt. TCPL <q...@tirupatisteel.com> wrote:
Please suggest electrode for welding sa516 & sa105

--

José Juan Jiménez Alejandro

unread,
Oct 29, 2020, 1:40:57 AM10/29/20
to material...@googlegroups.com
E7018 SMAW
ER70S-6 GMAW / GTAW

El mié., 28 de octubre de 2020 1:55 a. m., QA/QC Deptt. TCPL <q...@tirupatisteel.com> escribió:
Please suggest electrode for welding sa516 & sa105

--

Sunny Modi

unread,
Oct 29, 2020, 1:41:27 AM10/29/20
to material...@googlegroups.com
E7018

On Wed, 28 Oct, 2020, 1:25 pm QA/QC Deptt. TCPL, <q...@tirupatisteel.com> wrote:
Please suggest electrode for welding sa516 & sa105

--

Bien.ND | weldinginspections.net

unread,
Nov 6, 2020, 10:43:07 PM11/6/20
to Materials & Welding
I recommend the guideline >>> Welding Consumables guides in API RP 582 2016 - Welding Guidelines for the Chemical, Oil, and Gas Industries. Annex A: Table A.1 - Carbon and Low-alloy Steel
Reply all
Reply to author
Forward
0 new messages