Dissimilar welding of ASTM A182 F1 to Ferritic stainless steel grade 405

25 views
Skip to first unread message

RUSHABH PANJABI

unread,
May 12, 2016, 3:12:11 AM5/12/16
to Materials & Welding
Which filler wire to be used for such a dissimilar combination? and PWHT Condition.

Himan Nikdin

unread,
May 17, 2016, 5:18:23 AM5/17/16
to material...@googlegroups.com
as PWHT is mandatory  ENiCrFe-2 or -3 or ENiCrMo-3 can be used 


Date: Wed, 11 May 2016 23:39:51 -0700
From: rushabh...@gmail.com
To: material...@googlegroups.com
Subject: [MW:24785] Dissimilar welding of ASTM A182 F1 to Ferritic stainless steel grade 405


Which filler wire to be used for such a dissimilar combination? and PWHT Condition.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01ce5e86-8054-4639-9aad-a33b8f1fd279%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages